B-stage epoxy bonding · 9.5 mm diamonds · bonds at 105–120 °C

Diamond Dotted & Epoxy Prepreg Dotted paper and prepreg for bonded layer insulation

Diamond dotted paper and epoxy prepreg carry a B-stage epoxy printed in a diamond grid on kraft paper or polyester film. Under heat and pressure the resin flows, bonds the adjacent layers and closes the air voids that start partial discharge.

Diamond dotted insulation paper DDP for transformers
Diamond dotted insulation paper — 9.5 × 9.5 mm dots at 15.9 mm centres on 0.08–0.25 mm kraft base.
Diamond size
9.5 × 9.5 mm
Dot spacing
15.9 mm centres
Base thickness
0.08–0.25 mm
Bonding temperature
105–120 °C
Material range

Dotted and prepreg materials

Two families: diamond dotted paper and film for oil-immersed layer insulation, and epoxy prepreg for bonded rigid sections. Both are specified by base material, dot geometry and bonding cycle.

Selection and processing

Selecting and specifying Diamond Dotted and Epoxy Prepreg

  • Name the base and the thickness. Kraft paper 0.08–0.25 mm for oil-immersed layer insulation, or polyester film where a higher dielectric is wanted at the same build.
  • Give the bonding cycle your press can hold. The resin self-bonds at 105–120 °C; pressure and dwell decide whether the layer bonds without starving the bond line of resin.
  • Confirm the dot geometry. Standard is 9.5 × 9.5 mm diamonds at 15.9 mm centre-to-centre on a 960 mm base width; a different pattern has to be agreed before the resin is printed.
  • Agree how the bond is proven. A peel or delamination check on a cured sample, the resin flow figure, and the storage condition the roll will see before use.
How ordering works

From dotted paper specification to batch delivery

  1. 01 Send your specification

    Thickness, width, quantity, thermal class and the drawing or standard you work to.

  2. 02 Base and resin confirmed

    Base paper or film, thickness and dot pattern fixed; the bonding window is matched to your press cycle.

  3. 03 Cured sample approved

    A sample is bonded in your process and checked for delamination before the production roll is printed.

  4. 04 Production and batch test

    Batch run, test report and packing confirmed against the order before dispatch.

1986founded
22production lines
130+countries served
3,000+customers
Certified & audited: UL E310670 IATF 16949 ISO 9001 ISO 14001 CE RoHS REACH CNAS
Questions buyers ask

Diamond dotted and prepreg questions

At what temperature do the epoxy dots bond?

The B-stage resin self-bonds at 105–120 °C. Above that window the resin flows further and the bond line thins, so dwell and pressure are set from a cured sample rather than from the oven setting alone.

What is the standard dot pattern?

9.5 × 9.5 mm diamonds at 15.9 mm centre-to-centre spacing, printed on 960 mm wide kraft base paper or polyester film.

Can diamond dotted paper be used in oil-immersed transformers?

Yes. It is the standard layer insulation for oil-immersed windings: kraft base at Class A (105 °C) in oil, coated with B-stage epoxy so adjacent layers bond and the oil ducts stay free of voids.