6640 NMN Polyester Film/Polyaramide Fibre Paper Composite Insulation Paper

6640 NMN Polyester Film/Polyaramide Fibre Paper Composite Insulation Paper

This product has excellent electrical insulating properties, heat resistance, mechanical strength and impregnated property.

ISO 9001:2015 ISO 14001:2015 ISO 45001:2018 UL E310670 RoHS REACH

Description

This product has excellent electrical insulating properties, heat resistance, mechanical strength and impregnated property.   The properties (mechanical strength, breakdown voltage, flexibility and stiffness) of NMN are different for using different nominal thickness’ polyester film. The thickness of the polyester film should be clearly indicated in purchasing order or contract.  

Technical Specifications

Item Unit Requirement
Nominal thickness mm 0.15 0.17 0.19 0.22 0.24 0.26 0.31 0.37 0.41
Thickness tolerance mm ±0.022 ±0.024 ±0.026 ±0.031 ±0.037 ±0.041
Grammage g/m2 150±18 170±20 200±24 230±27 270±32 305±36 360±43 450±54 515±61
Film nominal thickness um 36 50 75 100 125 150 188 250 300
Tensile strength MD no bending N/10mm ≥150 ≥150 ≥170 ≥190 ≥220 ≥240 ≥270 ≥330 ≥370
MD after bending ≥90 ≥90 ≥105 ≥120 ≥150 ≥180 ≥200 ≥300 ≥330
TD no bending ≥80 ≥90 ≥100 ≥110 ≥130 ≥170 ≥200 ≥250 ≥300
TD after bending ≥70 ≥70 ≥90 ≥100 ≥120 ≥150 ≥150 ≥200 ≥230
Elongation (%) MD % ≥15 ≥3
TD ≥20 ≥10
Breakdown voltage No bending KV ≥7 ≥8 ≥11 ≥12 ≥14 ≥16 ≥19 ≥23 ≥25
After bending ≥6 ≥7 ≥9 ≥10 ≥12 ≥14 ≥15 ≥18 ≥19
Delamination — No Delamination, no bubble or other defects
Heat affected (180±2℃) 10min   No Delamination, no bubble, no adhesive flow
Long-term heat resistance (temperature index TI)   ≥155
Weight and area conversion m2/Kg 7.23 6.33 5.18 4.39 3.8 3.36 2.85 2.28 1.97

Specifications

Item Unit Requirement
Nominal thickness mm 0.15 0.17 0.19 0.22 0.24 0.26 0.31 0.37 0.41
Thickness tolerance mm ±0.022 ±0.024 ±0.026 ±0.031 ±0.037 ±0.041
Grammage g/m2 150±18 170±20 200±24 230±27 270±32 305±36 360±43 450±54 515±61
Film nominal thickness um 36 50 75 100 125 150 188 250 300
Tensile strength MD no bending N/10mm ≥150 ≥150 ≥170 ≥190 ≥220 ≥240 ≥270 ≥330 ≥370
MD after bending ≥90 ≥90 ≥105 ≥120 ≥150 ≥180 ≥200 ≥300 ≥330
TD no bending ≥80 ≥90 ≥100 ≥110 ≥130 ≥170 ≥200 ≥250 ≥300
TD after bending ≥70 ≥70 ≥90 ≥100 ≥120 ≥150 ≥150 ≥200 ≥230
Elongation (%) MD % ≥15 ≥3
TD ≥20 ≥10
Breakdown voltage No bending KV ≥7 ≥8 ≥11 ≥12 ≥14 ≥16 ≥19 ≥23 ≥25
After bending ≥6 ≥7 ≥9 ≥10 ≥12 ≥14 ≥15 ≥18 ≥19
Delamination — No Delamination, no bubble or other defects
Heat affected (180±2℃) 10min   No Delamination, no bubble, no adhesive flow
Long-term heat resistance (temperature index TI)   ≥155
Weight and area conversion m2/Kg 7.23 6.33 5.18 4.39 3.8 3.36 2.85 2.28 1.97